Aluminium Alloy Wires

Magnesium is the primary constituent in this alloy. AA is moderate strength, non-heat treatable alloy that combines its Strength with excellent Formability & Corrosion Resistance. Aluminum’s unique combination of properties makes it a highly versatile material when alloyed with various metals. Besides light weight characteristics and corrosion resistance property it’s excellent workability make it a natural choice for industrial use.

AA wires are used in many products by the leaders of the industry as raw material.

Specifications:

Diameter 0.12 mm – 6.00 mm”
Type (Modulus) Single Filar, Bifilar, Tri Filar, Tetra Filar (Quadri Filar)
Applications
  • Flexible cables
  • Coaxial cables
  • Wire used Electrical Appliances,
  • Water-Bottle Carver/parcel grids for bicycles
  • Mosquito Nets
  • Foodstuff Clips, Metal Staples (example for Sausage Type foods, Tea Bags}
  • Lightning Conductors
  • Clips, Staples for Staplers, Paper Clips
  • Clothes Pegs, Aluminium Clothes Hangers, usually used by Dry Cleaners
  • Refrigerator Grilles
  • Pipe Hose for Sanitary Fittings
  • Pipe Hose for Low Pressure Drinking Water, for Low Pressure Oil, Air and Petrol, Anti-vibration Tubes
  • Steel Deoxidizer In the Continuous Casting process
  • Shots
  • Rivets
GRADE SI % (max) FE % (max) CU % (max) MN % MG % CR. % ZN % (max) TI % Other (max) Aluminium
5019 0.40 0.50 0.10 0.10 – 0.60 4.50 – 5.60 0.20 (MAX) 0.20 0.20 (MAX) 0.15 Balance
5050 0.40 0.70 0.20 0.10 (MAX) 1.1- 1.8 0.10 (MAX) 0.25 0.15 Balance
5052 0.25 0.40 0.10 0.10 (MAX) 2.2- 2.8 0.15 – 0.35 0.15 Balance
5056 0.30 0.40 0.10 0.05 -0.20 4.50 – 5.60 0.05 -0.20 0.10 0.15 Balance
5154 0.45 0.45 0.10 0.80 – 1.30 2.80 – 3.50 0.20 0.20 (MAX) Balance
5356 0.25 0.40 0.10 0.05 -0.20 4.50 -5.50 0.050 – 0.20 0.10 0.06 – 0.20 0.15 Balance
5754 0.40 0.40 0.10 0.50 (MAX) 0.26 – 36 0.30 (MAX) 0.20 0.15 (MAX) 0.15 Balance
6101 0.3 – 0.7 0.5 0.10 0.03 (MAX) 0.35 -0.38 0.03 (MAX) 0.10 0.15 Balance
6201 0.60 0.22 0.007 0.63 (MAX) 0.004 (MAX) 0.008 NI 0.003 (MAX) PB 0.007 Balance
Normal Diameter Ω/mm Diameter difference ±mm Resistivity (20°C) < 0km/mm2 Measured (20°C) < 0/km Density (20°C) g/cm3 Conductivity (20°C) ≥ intensity test of the Soft state >N Tensile Strength of Soft-State >N mm2 Soft-state elongsion >N Bard Intensity >N Tensile Strength hard state >N mm2 Part enlongsion >N mm2
0.1 0.003 48 6111 2.78 36 1.6 210 8 2.6 340 1
0.11 0.003 48 5050 2.78 36 1.9 210 8 3.2 340 1
0.12 0.003 48 4244 2.78 36 2.3 210 8 3.8 340 1
0.13 0.003 48 3616 2.78 36 2.7 210 8 4.5 340 1
0.14 0.003 48 3118 2.78 36 3.2 210 8 5.23 340 1
0.15 0.003 48 2716 2.78 36 3.7 210 10 6 340 1
0.16 0.003 48 2387 2.78 36 4.2 210 10 6.8 340 1
0.17 0.003 48 2114 2.78 36 4.7 210 10 7.7 340 1
0.18 0.003 48 1886 2.78 36 5.3 210 10 8.6 340 1
0.19 0.003 48 1692 2.78 36 5.9 210 10 9.6 340 1
0.2 0.004 48 1527 2.78 36 6.5 210 10 10 340 1
0.25 0.004 48 977 2.78 36 10 210 12 16 340 1
0.3 0.004 48 679 2.78 36 14 210 12 24 340 1
0.35 0.004 48 498 2.78 36 20 210 12 32 340 1
0.4 0.005 48 381 2.78 36 26 210 12 42 340 1
0.45 0.005 48 301 2.78 36 33 210 12 54 340 1
0.5 0.005 48 244 2.78 36 41 210 12 66 340 1
0.64 0.006 48 149 2.78 36 67 210 12 109 340 1
0.7 0.007 48 124 2.78 36 80 210 12 130 340 1
0.81 0.008 48 93.1 2.78 36 108 210 12 175 340 1
0.9 0.009 48 75.4 2.78 36 133 210 12 216 340 1
1.02 0.01 48 58.7 2.78 36 171 210 12 277 340 1
1.13 0.011 48 47.8 2.78 36 210 210 12 340 340 1
1.38 0.013 48 32 2.78 36 314 210 12 508 340 1
1.63 0.016 48 23 2.78 36 438 210 12 709 340 1
1.78 0.017 48 19.2 2.78 36 522 210 12 846 340 1
1.96 0.019 48 15.9 2.78 36 633 210 12 1025 340 1